Precision Polymer Engineering P70B Polyacrylate Rubber
Subcategory: Elastomer, TS; Thermoset
Material Notes: Polyacrylic or Polyacrylate Rubber, 65-75 °IRHD. Copolymer of ethyl acrylate and vinyl ether. ASTM & ISO designation = ACM.Applications: Extensively used in automotive transmission systems. Superior resistance to heat and deterioration by hot hydraulic oil, when compared to nitrile rubber. Resistance to weathering and ozone is good, but resistance to water is relatively poor.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|