Precision Polymer Engineering S50E Silicone Rubber
Subcategory: Silicone; Elastomer, TS; Thermoset
Material Notes: Red iron oxide filled, Phenyl Silicone Rubber, 45-55 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Specification DTD818 Class M2. ASTM & ISO designation = PVMQ.Applications: Excellent heat resistance plus ultra-low temperature flexibility. Used primarily for dry heat static seals. Low physical strength and poor abrasion resistance prevents dynamic sealing. Although silicone will swell in petroleum lubricants, this is not necessarily detrimental in static sealing applications.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,