Precision Polymer Engineering S50T Silicone Rubber
Subcategory: Silicone; Elastomer, TS; Thermoset
Material Notes: Translucent Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and low temperature flexibility. Used primarily for dry heat static seals, (the low physical strength and poor abrasion resistance prevents dynamic sealing).