Precision Polymer Engineering S55T Silicone Rubber
Subcategory: Silicone; Elastomer, TS; Thermoset
Material Notes: Translucent Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations, Title 21 (CFR21), Section 177.2600. Extraction tested. Compliant to BGA XVA and KTW 1.3.13. ASTM & ISO designation = VMQ.Applications: Excellent mechanical, physical and chemical stability over the temperature range of -40º to +180ºC. Excellent behaviour when sterilised. Intended for food contact, pharmaceutical and biomedical applications.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Extraction Test, 21 CFR 177.2600
- Low Temperature Resistance, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|