Precision Polymer Engineering S60N Silicone Rubber
Subcategory: Silicone; Elastomer, TS; Thermoset
Material Notes: Red Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Grade 60.Applications: Particularly suitable in fluid sealing applications where low compression set is of prime importance in O-rings and gaskets. Can be used in contact with heavy mineral and certain diester-based oils within the quoted temperature range. Unsuitable for use in contact with petroleum based fuels, light mineral oils or greases derived from them. Excellent ozone resistance.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|