Premix Thermoplastics PRE-ELEC® CP 1316
Subcategory: Polyolefin; Additive/Filler for Polymer; Thermoplastic
Material Notes: PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity PRE-ELEC CP 1316 has good mechanical properties and is easy to extrude or injection mould.Typical applications include flexible extruded profiles and tubes and flexible injection molded parts. PRE-ELEC CP 1316 may also be used as a masterbatch and blended with EVA or PE-LD. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod. Information provided by Premix Thermoplastics Inc.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Middle Barrel Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
- Roll Temperature
- Dry Time
- Moisture Content
- Injection Pressure
- Appearance
- Color
- Injection Speed
- Storage Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|