Premix Thermoplastics PRE-ELEC® CP 1317

 

Subcategory: Ethylene Vinyl Acetate; Additive/Filler for Polymer; Thermoplastic; Polymer

Material Notes:
PRE-ELEC CP 1317 is a conductive thermoplastic compound based on EVA. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC CP 1317 has excellent mechanical properties and is suitable for film blowing. It is also suitable for coextrusion applications.

Typical applications include blown film for the production of bags for electronic components and other products that are sensitive to static electricity.

Information provided by Premix Thermoplastics Inc.

Available Properties
  • Density
  • Thickness
  • Melt Flow
  • Film Tensile Strength at Yield, MD
  • Film Tensile Strength at Yield, TD
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Film Elongation at Yield, MD
  • Film Elongation at Yield, TD
  • Surface Resistance
  • Melt Temperature
  • Blow-up Ratio (BUR)
  • Dry Time
  • Moisture Content
  • Appearance
  • Color
  • Screen Pack
  • Storage Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。