Premix Thermoplastics PRE-ELEC® ESD 5100

 

Subcategory: Polypropylene; Additive/Filler for Polymer; Thermoplastic

Material Notes:
PRE-ELEC ESD 5100 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 5100 can be injection molded, extruded, blow molded and blown into film. The products made out of PRE-ELEC ESD 5100 are washable, reusable and recyclable. Surface resistance values of 108 ohms (EOS/ESD S11.11-1993, IEC 61340-5-1) can be achieved with optimum processing parameters.

Typical applications include tote bins, trays, bottles and bags which give permanent ESD protection for the electronics, medical, pharmaceutical and agricultural industries. PRE-ELEC ESD 5100 can be colored into various bright colors.

Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod.

Information provided by Premix Thermoplastics Inc.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Modulus of Elasticity
  • Izod Impact, Notched (ISO)
  • Izod Impact, Unnotched
  • Surface Resistance
  • Static Decay
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Flammability, UL94
  • Middle Barrel Temperature
  • Die Temperature
  • Melt Temperature
  • Mold Temperature
  • Roll Temperature
  • Dry Time
  • Moisture Content
  • Injection Pressure
  • Appearance
  • Color
  • Injection Speed
  • Storage Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。