Premix Thermoplastics PRE-ELEC® ESD 7200
Subcategory: Polycarbonate; ABS Polymer; Additive/Filler for Polymer; Thermoplastic
Material Notes: PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for injection molding. The products made out of PRE-ELEC ESD 7200 are washable, reusable and recyclable. Surface resistance values of 108 ohms (EOS/ESD S11.11-1993, IEC 61340-5-1) can be achieved with optimum processing parameters.Typical applications include injection molded technical parts used in e.g. office machines, telecommunication, electronics, medical and pharmaceutical industries, which give permanent ESD protection. PRE-ELEC ESD 7200 can also be extruded into sheets for thermoforming. Information provided by Premix Thermoplastics Inc.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Modulus of Elasticity
- Izod Impact, Unnotched
- Izod Impact, Notched
- Surface Resistance
- Static Decay
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Middle Barrel Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
- Roll Temperature
- Dry Time
- Moisture Content
- Appearance
- Color
- Injection Pressure
- Injection Speed
- Post Pressure, psi
- Storage Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|