Premix Thermoplastics PRE-ELEC® PA 1406
Subcategory: Nylon; Additive/Filler for Polymer; Thermoplastic; Nylon 6
Material Notes: PRE-ELEC PA 1406 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon fiber. In addition to a low electrical resistivity PRE-ELEC PA 1406 has an excellent balance of mechanical properties and is easy to injection mould.Typical applications include injection molded technical parts and housings for electronic components and other static sensitive devices (SSD) when high rigidity is needed. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod. Information provided by Premix Thermoplastics Inc.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Melt Temperature
- Mold Temperature
- Dry Time
- Moisture Content
- Injection Pressure
- Appearance
- Color
- Injection Speed
- Storage Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|