Premix Thermoplastics PRE-ELEC® PE 1270
Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic; LLDPE
Material Notes: PRE-ELEC PE 1270 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 1270 has excellent mechanical properties and is easy to injection mould. Typical applications include injection molded technical parts where good impact strength in low temperatures is needed. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod. Information provided by Premix Thermoplastics Inc.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Vicat Softening Point
- Melt Temperature
- Mold Temperature
- Dry Time
- Moisture Content
- Injection Pressure
- Appearance
- Color
- Injection Speed
- Storage Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|