Premix Thermoplastics PRE-ELEC® PE 1290
Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic; HDPE; Polymer
Material Notes: PRE-ELEC PE 1290 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 1290 has an excellent balance of mechanical properties.Typical applications include extrusion of pipe and sheet which need good resistance to chemicals and blow molding of bottles, canisters and drums. Information provided by Premix Thermoplastics Inc.
| Available Properties |
- Density
- Thickness
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Yield, MD
- Film Elongation at Yield, TD
- Elongation at Break
- Modulus of Elasticity
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Middle Barrel Temperature
- Die Temperature
- Roll Temperature
- Dry Time
- Moisture Content
- Appearance
- Color
- Storage Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|