Premix Thermoplastics PRE-ELEC® PE 1295

 

Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic; HDPE

Material Notes:
PRE-ELEC PE 1295 is a dissipative thermoplastic compound based on PE-HD. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resistance between 106-109 ohms PRE-ELEC PE 1295 has an excellent balance of mechanical properties and is easy to injection mould.

Typical applications include injection molded pallets, crates, boxes and tote bins for electronic, automotive and chemical industry to prevent static charges.

Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod.

Information provided by Premix Thermoplastics Inc.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Modulus of Elasticity
  • Izod Impact, Notched (ISO)
  • Izod Impact, Unnotched (ISO)
  • Volume Resistivity
  • Surface Resistance
  • Static Decay
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Melt Temperature
  • Mold Temperature
  • Dry Time
  • Injection Pressure
  • Injection Speed
  • Storage Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。