Premix Thermoplastics PRE-ELEC® PP 1395
Subcategory: Polypropylene; Additive/Filler for Polymer; Thermoplastic
Material Notes: PRE-ELEC PP 1395 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resistance between 106-109 ohms PRE-ELEC PP 1395 has an excellent balance of mechanical properties and is easy to injection mould.Typical applications include injection molded crates, boxes, pallets and tote bins for electronic, automotive and chemical industry to prevent static charges. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod. Information provided by Premix Thermoplastics Inc.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Modulus of Elasticity
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched (ISO)
- Volume Resistivity
- Surface Resistance
- Static Decay
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Melt Temperature
- Mold Temperature
- Dry Time
- Injection Pressure
- Injection Speed
- Storage Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|