Premix Thermoplastics PRESEAL TPE 6070
Subcategory: Elastomer, TPE; Additive/Filler for Polymer; Thermoplastic
Material Notes: PRESEAL TPE 6070 is a novel thermoplastic elastomer based highly conductive compound intended primarily for EMI gasketing and grounding applications. Conductivity is achieved with a silver coated glass sphere and fiber combination. PRESEAL TPE 6070 can be injection molded like an ordinary thermoplastic elastomer thus giving great new possibilities in gasket design and mass production. It has adhesion to selected thermoplastics and insert molding to metal is also possible. This opens interesting construction possibilities with co-injection molding e.g. molding the gasket directly in the phone casing. Recyclability is an added value. The material is silicone free.Typical applications include soft EMI gaskets in mobile phones, mobile phone base stations and other wireless communication environment as well as military applications. * Tension test bar according to ISO 527 Information provided by Premix Thermoplastics Inc.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Modulus of Elasticity
- Compressive Modulus
- Tear Strength
- Compression Set
- Volume Resistivity
- Shielding Effectiveness
- Middle Barrel Temperature
- Nozzle Temperature
- Injection Velocity
- Dry Time
- Moisture Content
- Hold Pressure
- Back Pressure
- Appearance
- Color
- Cooling Time, sec
- Holding Time, sec
- Injection Time, sec
- Plasticizing Speed, %
- Storage Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|