Premix Thermoplastics PREBLACK PE 710-03
Subcategory: Additive/Filler for Polymer; Thermoplastic
Material Notes: PREBLACK PE 710-03 black color concentrate has been developed for extrusion coating applications where the use of a compound is preferred. The homogeneity of PREBLACK PE 710-03 is good with a low moisture absorption. The sulphur content of the carbon black is very low preventing odor problems. PREBLACK PE 710-03 can also be used for tinting. According to BgVV regulations PREBLACK PE 710-03 is approved for use in contact with foodstuffs, as long as the carbon black level in the produced product is less than 2.5 %. Information provided by Premix Thermoplastics Inc.
| Available Properties |
- Density
- Maximum Service Temperature, Air
- Moisture Content
- Appearance
- Carrier
- Light Fastness
- Pigmentation, %
- Storage Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|