Premix Thermoplastics PREBLACK PE 710-30
Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic
Material Notes: PREBLACK PE 710-30 is a polyethylene based black masterbatch for extrusion coating applications Due to the well-dispersed carbon black in PREBLACK PE 710-30 it has a very good hiding power and UV-resistance already at low dosing levels. The moisture absorption and sulphur content of PREBLACK PE 710-30 are low preventing unnecessary odor problems. According to BgVV regulations PREBLACK PE 710-30 is approved for use in contact with foodstuffs, as long as the carbon black level in the product produced is less than 2.5 %. Information provided by Premix Thermoplastics Inc.
| Available Properties |
- Density
- Maximum Service Temperature, Air
- Moisture Content
- Appearance
- Carrier
- Dosing, %
- Light Fastness
- Pigmentation, %
- Storage Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|