Premix Thermoplastics PREWHITE PE 10-50
Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic
Material Notes: PREWHITE PE 10-50 is a polyethylene based white masterbatch, well suited for the coloring of PE-LD and PE-HD films, profiles, hollow articles and injection molded goods. PREWHITE PE 10-50 can also be used for PP.Films can be blown down to 20 microns due to the good dispersion of PREWHITE PE 10-50. According to FDA and BgVV regulations PREWHITE PE 10-50 is approved for use in contact with foodstuffs without limitations. Information provided by Premix Thermoplastics Inc.
| Available Properties |
- Density
- Additive Loading
- Maximum Service Temperature, Air
- Moisture Content
- Appearance
- Carrier
- Dosing, %
- Light Fastness
- Storage Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|