Premix Thermoplastics PREWHITE PP 51-50
Subcategory: Polypropylene; Additive/Filler for Polymer; Thermoplastic
Material Notes: PREWHITE PP 51-50 is a polypropylene based white masterbatch developed for the coloring of PP cast and BOPP films plus extruded polypropylene sheets.Due to very good homogeneity of PREWHITE PP 51-50, it is well suited for fast line speeds, thin layers and relatively high masterbatch dosages. According to FDA and BgVV regulations PREWHITE PP 51-50 is approved for use in contact with foodstuffs without limitations. Information provided by Premix Thermoplastics Inc.
| Available Properties |
- Density
- Additive Loading
- Maximum Service Temperature, Air
- Moisture Content
- Appearance
- Carrier
- Dosing, %
- Light Fastness
- Storage Time
|
|
|
|