Premix Premi-Glas® 1205 Glass Reinforced SMC
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Material Notes: Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: - Excellent warp resistance and dimensional repeatability
- Excellent resistance to sagging and distortion during door skin assembly
- Very good flow and fill in thin moldings
- Outstanding appearance in wood-grain textured or smooth surface applications
- Standard colors are beige and white
Market: Construction/Residential Doors Information provided by Premix.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Poissons Ratio
- Izod Impact, Unnotched
- Izod Impact, Notched
- CTE, linear 68°F
- CTE, linear 68°F, Transverse to Flow
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|