Premix Premi-Glas® 1261-28 VE Glass Reinforced Vinyl Ester TMC
Subcategory: Vinyl Ester; Composite SMC; Thermoset; Polymer
Material Notes: Description: Premi-Glas® 1261-28 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: - Excellent thermal stability and resistance to the corrosive effects of automotive fluids
- Excellent flow at moderate pressures, allowing easy molding in complex geometries
- Designed for Injection or Injection-Compression molding
- Replaces Cast Metals for reduced Noise, Vibration, and Harshness, plus molded-in color
- TMC compounding process preserves glass integrity for excellent strength vs. BMC
Market: Composite PowerTrain Information provided by Premix.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Poissons Ratio
- Izod Impact, Unnotched
- Dielectric Strength
- CTE, linear 68°F
- CTE, linear 68°F, Transverse to Flow
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|