Premix Premi-Glas® 1265-VE (Compression Molded) Glass Reinforced Vinyl Ester TMC
Subcategory: Vinyl Ester; Composite SMC; Thermoset; Polymer
Material Notes: Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: - Designed for Injection or Injection-Compression molding
- Excellent resistance to automotive chemicals and fluids, and to salt spray
- Replaces Cast Metals for reduced Noise, Vibration and Harshness, plus molded-in color
- TMC compounding process preserves glass integrity for excellent strength vs. BMC
- Excellent thermal properties and elevated temperature modulus retention
- Mechanical data below are from compression-molded panels as required for certain specifications; see separate data sheet for injection-compression values
Market: Composite PowerTrain Information provided by Premix.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Poissons Ratio
- Izod Impact, Unnotched
- CTE, linear 68°F, Transverse to Flow
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|