Premix Premi-Glas® 2200-25 CR-SX Fiberglass Reinforced SMC
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Material Notes: Description: Premi-Glas® 2200-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and dimensional stability, and corrosion resistance. Key features and benefits: - Underwriters Laboratories 945VA flame resistance at 1.5 mm minimum wall thickness
- Subjected to UL746C testing for consideration in exterior applications involving ultraviolet light and water immersion or humidity exposure
- Formulated for moderate shrinkage to permit good dimensional stability while releasing from deep-draw moldings
- Refer to UL file E42524.
Market: Electrical/Flame Retardant Information provided by Premix.
| Available Properties |
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Poissons Ratio
- Izod Impact, Unnotched
- Izod Impact, Notched
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 68°F
- CTE, linear 68°F, Transverse to Flow
- Specific Heat Capacity
- Thermal Conductivity
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|