Premix Premi-Glas® 8105 Glass Reinforced Polyester BMC
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Material Notes: Description: Premi-Glas® 8105 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: - Excellent dimensional stability and heat resistance
- Faster molding cycle times vs. Premi-Glas® 8101
- Designed for high speed, automated injection molding processes
- Improved adhesion vs. Premi-Glas® 8101 with UV-curable basecoats
- Meets the requirements of GM GMP.UP.014 and Ford WSB-M3D171-A1
- Available in grey color
Market: Forward Lighting Information provided by Premix.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Poissons Ratio
- Izod Impact, Unnotched
- Izod Impact, Notched
- CTE, linear 68°F
- CTE, linear 68°F, Transverse to Flow
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|