Premix Premi-Glas® 8201-24 Glass Reinforced Polyester SMC
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Material Notes: Description: Premi-Glas® 8201-24 is a low profile glass reinforced polyester Sheet Molding Compound designed for body panel applications.Key features and benefits: - Compatible with in-mold coatings, in-mold powder coatings, and many automotive primers
- Excellent flow and fill in complex molding geometries
- Molds well in deep-draw parts as well as in thin-skin moldings
- Automotive Class A surface profile; minimal short and long term waviness
- Used in body panel applications in transportation, recreational, and marine applications
Market: Consumer/Recreational Information provided by Premix.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Poissons Ratio
- Izod Impact, Unnotched
- Izod Impact, Notched
- CTE, linear 68°F
- CTE, linear 68°F, Transverse to Flow
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|