Premix Premi-Glas® 2205-20 CRSX Polyester SMC

 

Subcategory: Composite SMC; Polyester, TS; Thermoset

Key Words: Sheet Molding Compound

Material Notes:
Premi-Glas® 2205-20 CR-SX is a 20% fiberglass reinforced Sheet Molding Compound formulated for condensate pan applications requiring chemical resistance, heat resistance, dimensional stability, weatherability, and mechanical property retention following long term heat exposure. Key features and benefits are:

  • Recognized by Underwriters Laboratory, UL 94-5VA flame recognition at 2.54mm minimum wall thickness and UL 94 V0 flame recognition at 1.78mm. minimum wall thickness.
  • UL recognized in all colors.
  • Formulated to provide accurate as-molded dimensional tolerances.
  • Meets stringent UL-484 requirements for acceptability in room air conditioners following testing for retention of mechanical /electrical properties after UV exposure, water emersion, and oven aging tests.
  • Carries UL 746C recognition for acceptability for outdoor use following UV light, water exposure, and immersion testing.

Data provided by Premix.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Tensile Strength, Ultimate
  • Modulus of Elasticity
  • Flexural Modulus
  • Flexural Yield Strength
  • Izod Impact, Unnotched
  • Izod Impact, Notched
  • Dielectric Strength
  • Arc Resistance
  • Track Resistance
  • Deflection Temperature at 1.8 MPa (264 psi)
  • UL RTI, Electrical
  • UL RTI, Mechanical with Impact
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。