Premix Premi-Glas® 2205-20 CRSX Polyester SMC
Subcategory: Composite SMC; Polyester, TS; Thermoset
Key Words: Sheet Molding Compound
Material Notes: Premi-Glas® 2205-20 CR-SX is a 20% fiberglass reinforced Sheet Molding Compound formulated for condensate pan applications requiring chemical resistance, heat resistance, dimensional stability, weatherability, and mechanical property retention following long term heat exposure. Key features and benefits are:- Recognized by Underwriters Laboratory, UL 94-5VA flame recognition at 2.54mm minimum wall thickness and UL 94 V0 flame recognition at 1.78mm. minimum wall thickness.
- UL recognized in all colors.
- Formulated to provide accurate as-molded dimensional tolerances.
- Meets stringent UL-484 requirements for acceptability in room air conditioners following testing for retention of mechanical /electrical properties after UV exposure, water emersion, and oven aging tests.
- Carries UL 746C recognition for acceptability for outdoor use following UV light, water exposure, and immersion testing.
Data provided by Premix.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Dielectric Strength
- Arc Resistance
- Track Resistance
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|