Premix Premi-Glas® 2100-10CRSX Polyester BMC

 

Subcategory: Polyester, TS; Thermoset

Material Notes:
Premi-Glas® 2100-10 CR-SX is a 10% fiberglass reinforced Bulk Molding Compound formulated for applications requiring excellent chemical resistance, thermal resistance, dimensional stability and weatherability characteristics. Key features and benefits are:

  • Underwriters Laboratory, U.L. 94-5VA & U.L. 94 V0 flame recognition at 1.47mm minimum wall thickness.
  • U.L. flame recognition in all colors.
  • Available in fiberglass content of 10-30%.
  • Formulated to provide accurate as-molded dimensional tolerances.
  • The Premi-Glas 2100 CR-SX series SMC carries U.L. 746C recognition for use in exterior applications following ultraviolet light, water emersion and exposure testing.
  • Typical applications include outdoor use in light housings, reflectors and electrical enclosure products.

Data provided by Premix.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Tensile Strength, Ultimate
  • Modulus of Elasticity
  • Flexural Modulus
  • Flexural Yield Strength
  • Izod Impact, Unnotched
  • Izod Impact, Notched
  • Dielectric Strength
  • Arc Resistance
  • Track Resistance
  • Deflection Temperature at 1.8 MPa (264 psi)
  • UL RTI, Electrical
  • UL RTI, Mechanical with Impact
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。