Professional Plastics Kaptrex® Polyimide Film
Subcategory: Polyimide, TS; Thermoset; Polymer
Material Notes: Kaptrex PI film provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. Kaptrex polyimide film provides excellent electrical properties and resistance to high temperature and radiation. It is suitable for insulation of “H” class (180°C or 356°F) electrical machines and appliances under working temperature of 200°C(392°F). Availability: Thickness from .001” up to .005” Widths: Standard Rolls for 24.5” wide. Applications: Wire Wrap Insulation & Tapes, Flexible Printed Circuits, Motor Slot Liners, Pressure Sensitive Tapes, Aerospace Shims, Formed Coil Insulation.
| Available Properties |
- Density
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|