Chevron EA6025 Rubber Modified Polystyrene
Subcategory: Polystyrene; Thermoplastic
Key Words: PS
Material Notes: Description Chevron EA5025 is a high impact polystyrene resin developed for custom sheet extrusion. It offers excellent extrusion and thermoforming characteristics, practical toughness, and good surface gloss. Chevron EA6025 natural complies with Food Additive Regulation 21CFR177.1640 for polystyrene and rubber modified polystyrene, which states that such materials may be safely used in contact with foods. Applications Chevron EA6025 is recommended for such applications as point of purchase displays, food service trays, shower surrounds and liners.Information provided by Chevron Phillips Chemical Company.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Izod Impact, Notched, Low Temp
- Izod Impact, Notched
- Vicat Softening Point
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|