Chevron MC3600 High Flow Crystal Polystyrene

 

Subcategory: Polystyrene; Thermoplastic

Key Words: PS

Material Notes:
Description

Chevron polystyrene resin MC3600 crystal is an easy flowing, crystal clear polystyrene injection molding compound, designed specifically for thin- and medium-walled parts of any size or complexity. MC3600 combines greater processing latitude, exceptional mold release and the overall good molding characteristics required by such parts. MC 3600 provides improved cycle times, better stackability, reduced dusting and fewer part rejects. Processing energy requirements can also be reduced. Chevron MC3600 crystal complies with Food Additive Regulation 21CFR177.1640 for polystyrene and rubber modified polystyrene, which states that such materials may be safely used in contact with foods.

Applications

Housewares, disposable cups and cutlery are typical applicationsInformation provided by Chevron Phillips Chemical Company.

Available Properties
  • Density
  • Melt Flow
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。