IDI C-105 Thermoset Polyester, Molding
Subcategory: Polyester, TS; Thermoset
Close Analogs: 18 IDI molding grade polyesters are listed in MatWeb. Data provided by the manufacturer.
Key Words: Industrial Dielectrics Inc.; BMC
Material Notes: Vinylester compounds in a range of strengths with superior corrosion resistance.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Flammability, UL94
|
|
|
|