IDI A-203 Thermoset Polyester, Sheet
Subcategory: Composite SMC; Polyester, TS; Thermoset
Close Analogs: 16 IDI sheet grade polyesters are listed in MatWeb. Data provided by the manufacturer.
Key Words: Industrial Dielectrics Inc.; SMC
Material Notes: AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion resistance. Excellent paintability.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Dielectric Strength
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|