Pyrotek TS-81 Thermoset Electrical Insulation Product (Nema Grade: CE)
Subcategory: Phenolic; Thermoset; Polymer
Material Notes: Cotton reinforcement, Phenolic resin, Natural / Tan color. Economy grade. Good acid resistance. Applications - Superstructure support pads
- Bus bar insulators
- Pot cradle insulators
- Exhaust duct insulators
- Machined parts
- Wedges & shunts
- Point feeder gaskets
Advantages - High insulation properties
- High strength
- Low moisture absorption
- High temperature resistance
Information provided by Pyrotek.
| Available Properties |
- Density
- Water Absorption
- Flexural Strength
- Compressive Strength
- Dielectric Strength
- Maximum Service Temperature, Air
|
|
|
|