|   Pyrotek TS-85 Thermoset Electrical Insulation Product (Nema Grade: L)  Subcategory: Phenolic; Thermoset; Polymer Material Notes: Linen reinforcement, Phenolic resin, Natural color.  Good mechanical strength.  Good machining qualities.
 Information provided by Pyrotek. 
| | 
    | Available Properties |  
    | DensityWater AbsorptionFlexural StrengthCompressive StrengthDielectric StrengthMaximum Service Temperature, Air
 | 
 | 
 |  | | 
    | Property Data |  
    | 