Pyrotek F-24 Dense Machinable Board
Subcategory: Thermoset; Polymer
Material Notes: F-24 is a high temperature resin material that is reinforced with fiberglass. Abrasion resistant, it is used for hot glass handling applications. Applications - Donut rollers for glass
- Guide rails
- Wear pads
- Machined insulators
Advantages - Abrasion resistant
- Excellent heat resistance
- Non-marking to glass
- Economical
- Easily machined
- Good physical strength
- Excellent wear resistance
- Good shock resistance
Information provided by Pyrotek.
| Available Properties |
- Tensile Strength, Ultimate
- Flexural Strength
- Compressive Strength
- Shear Strength
- Izod Impact, Notched
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|