Pyrotek TS-550 Insulating Board

 

Subcategory: Phenolic; Thermoset; Polymer

Material Notes:
TS-550 is phenolic-based, fiber and mineral reinforced, high-temperature material. TS-550 offers the high strength and wear resistant properties of laminated materials, while also offering the forming versatility and uniform material composition of engineering plastics.

Applications

  • Container glass pad material
  • Glass conveyor rollers and guides

Advantages

  • Extremely wear resistant
  • Low porosity prevents oil absorption
  • Low thermal conductivity
  • Capable of being machined or molded into exceptionally high tolerance parts

Information provided by Pyrotek.

Available Properties
  • Density
  • Water Absorption
  • Flexural Strength
  • Compressive Strength
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。