Qualchem Danamid AFEM-5 Polyamide 66, 5% MoS2
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes: With MoS2, decreased friction propertiesInformation provided by Qualchem Zrt.
| Available Properties |
- Filler Content
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Moisture Content
|
|
|
|
| Property Data |