Qualchem Danaprop PP2GF-15 Polypropylene, 15% Glass Fiber
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Polypropylene (homo-polymer) reinforced with glass fiberInformation provided by Qualchem Zrt.
| Available Properties |
- Filler Content
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|