RTP Company RTP 307 SE Polycarbonate (PC) Glass Fiber - Self Extinguishing - Halogen Free - UL94 V-2
Subcategory: Polycarbonate; Thermoplastic
Material Notes: The RTP 300 SE series represent a range of glass fiber reinforced, self-extinguishing polycarbonate materials which offer outstanding dimensional stability with improved rigidity, heat resistance and strengths over the base resin.
| Available Properties |
- Specific Gravity
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Moisture Content
- Dew Point
- Injection Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|