RTP Company RTP 303 FR UV Polycarbonate (PC) Glass Fiber - Flame Retardant - Non-PBBO/E - UV Stabilized
Subcategory: Polycarbonate; Thermoplastic
Material Notes: The RTP series of flame retardant, glass fiber reinforced polycarbonate materials offer dimensional stability with improved heat distortion and ignition resistance performance over the base resin. RTP 303 FR UV includes additional stabilization against UV degradation.
| Available Properties |
- Specific Gravity
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Moisture Content
- Dew Point
- Injection Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|