RTP Company RTP 301 TFE 15 FR L Polycarbonate (PC) Glass Fiber - PTFE Lubricated - Flame Retardant - Non-PBBO/E - UL94 V-0
Subcategory: Polycarbonate; Thermoplastic
Material Notes: The RTP 301 TFE FR L series of compounds incorporate various percentages of PTFE into a glass fiber reinforced polycarbonate base which also includes external lubricants for enhanced processing. These UL94 V-0 certified materials exhibit excellent dimensional stability, low wear characteristics with enhanced strength and heat resistance.
| Available Properties |
- Specific Gravity
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Moisture Content
- Dew Point
- Injection Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|