RTP Company RTP 1004 FR A Polybutylene Terephthalate (PBT) Glass Fiber - Flame Retardant - UL94 V-0
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Material Notes: RTP 1001 - 1005 FRA are a series of glass fiber reinforced, flame retardant PBT compounds. All are UL94 V-0 certified down to the 1/32" (0.8mm) thickness. These materials exhibit easy flow, excellent physical properties and good processing characteristics.
| Available Properties |
- Specific Gravity
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Moisture Content
- Dew Point
- Injection Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|