RTP Company RTP 136 HB Polypropylene (PP) Mineral - UL94 HB
Subcategory: Polypropylene; Thermoplastic
Material Notes: RTP 136 HB is a mineral reinforced polypropylene offering improved stiffness, hardness, and heat distortion temperature vs. unreinforced polypropylene. It also exhibits lower shrinkage and better dimensional stability.
| Available Properties |
- Specific Gravity
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Injection Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|