RTP Company RTP 150 HI LF Polypropylene (PP) Flame Retardant - Living Hinge Grade - High Impact - Low Flow
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: Flame Retardant - Living Hinge Grade - High Impact - Low Flow Comments: - Flame Retardant
- Living Hinge Grade
- High Impact
- Low Flow
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, 6.35 mm section
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 68°F
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Mold Temperature
- Injection Pressure
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|