RTP Company RTP 203B GB 20 TFE 10 HS UV Nylon 6/10 (PA 6/10) Glass Fiber 20% - Glass Bead 20% - PTFE 10% - Heat Stable - UV Stable
Subcategory: Nylon; Thermoplastic; Nylon 610
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: Glass Fiber 20% - Glass Bead 20% - PTFE 10% - Heat Stable - UV Stable Comments: - Glass Fiber
- Glass Bead
- PTFE Lubricated
- Heat Stabilized
- UV Stabilized
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
| Available Properties |
- Specific Gravity
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, 6.35 mm section
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Electrical Resistivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Mold Temperature
- Injection Pressure
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|