|   RTP Company RTP 201D GB 20 Nylon 6/12 (PA 6/12) Glass Fiber 10% - Glass Bead 20%  Subcategory: Nylon; Thermoplastic; Nylon 612 Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
 Material Notes: Glass Fiber 10% - Glass Bead 20%
 Comments: Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company. 
| | 
    | Available Properties |  
    | Specific GravityFiller ContentWater AbsorptionLinear Mold ShrinkageLinear Mold Shrinkage, 6.35 mm sectionHardness, Rockwell RTensile Strength, UltimateElongation at BreakModulus of ElasticityFlexural ModulusFlexural Yield StrengthCompressive Yield StrengthIzod Impact, UnnotchedIzod Impact, NotchedElectrical ResistivityDielectric ConstantDielectric StrengthDissipation FactorCTE, linear 68°FThermal ConductivityDeflection Temperature at 0.46 MPa (66 psi)Deflection Temperature at 1.8 MPa (264 psi)Flammability, UL94Processing TemperatureMold TemperatureInjection PressureColor
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |