|   RTP Company RTP 207.3F Nylon 12 (PA 12) Glass Fiber 43%  Subcategory: Nylon; Thermoplastic; Nylon 12 Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
 Material Notes: Glass Fiber 43%
 Comments: Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company. 
| | 
    | Available Properties |  
    | Specific GravityFiller ContentLinear Mold ShrinkageTensile Strength, UltimateElongation at BreakModulus of ElasticityFlexural ModulusFlexural Yield StrengthIzod Impact, UnnotchedIzod Impact, NotchedFlammability, UL94Processing TemperatureMold TemperatureInjection PressureColor
 | 
 | 
 |  | | 