RTP Company RTP 4700 TFE 18 SI 2 Polytrimethylene Terephthalate (PTT) PTFE 18% - Silicone 2%
Subcategory: Polyester, TP; Thermoplastic; Polytrimethylene Terephthalate (PTT)
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: PTFE 18% - Silicone 2% Comments: - PTFE Lubricated
- Silicone Lubricated
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Mold Temperature
- Injection Pressure
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|