RTP Company ESD A 2800-55A Olefinic Thermoplastic Elastomer (TEO) Dissipative - 55 Shore A
Subcategory: Elastomer, TPE; Thermoplastic; Olefinic TPE
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: Dissipative - 55 Shore A Comments: - Static Dissipative
- ESD Protection
- 55-A Durometer
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Izod Impact, Unnotched
- Izod Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Static Decay
- Flammability, UL94
- Processing Temperature
- Mold Temperature
- Injection Pressure
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|